Hastelloy C22 plate

 

JN Alloy is largest Stockiest of Hastelloy C22 Plate supplier with huge inventory of Alloy C22 Hot Rolled Plate, ASTM B575 UNS N06022 Polished Plate and Hastelloy C22 Cold Rolled Plate. We offer Din 2.4602 Coils in various sizes at best price. We are leading manufacturer of Alloy C22 strip & Hastelloy C22 Sheet.

 

One of the most commonly used alloys the Hastelloy C22 Sheet may be used up to a temperature of 1250 °F. Using the alloy above 1250 °F could be harmful. It would give rise to detrimental phases in the alloy of the ASTM B575 Hastelloy C22 Alloy Plate. Most hastelloys are high temperature alloys. Mainly because the function well despite the exposure to elevated temperature settings. Yet, this nickel alloy is well suited for use in highly aggressive environments, including sour well and for processes such as flue-gas desulfurization. The alloy is resistant to reductive acids, so the Nickel Alloy C22 Plate could be used in industries that employ both sulfuric acid and hydrochloric acid. The inclusion of nickel, chromium and molybdenum elements in the Hastelloy C22 Cold Rolled Sheet is what gives them their primary attributes of which are resistance to not only oxidizing media but also against non-oxidizing chemicals. Moreover, the ASTM B575 UNS N06022 Strip also offers protection from localized corrosion attack such as pitting and crevice corrosion. Furthermore, according to the ASTM B575 specification, any nickel based alloy sheet, in this case, Alloy C22 Sheet must also conform to the grain size as mentioned in the specification besides the mechanical properties and chemical composition.

 

JN Alloys is Epitome in supplying, trading and manufacturing an extensive collection of Hastelloy C-22 Sheet to the respected customers. We also offer these Hastelloy Plates at best possible rates. Further, to make sure in their blemish free design, we inspect these Hastelloy Coils on predefined quality constraints. Meanwhile, these Hastelloy Slatting Coils are manufactured and designed at our high-tech manufacturing unit, which is fixed by means of strictly cutting – edge amenities and machines. We also offer these products in different grades such as Hastelloy C-22 Plates, Hastelloy C22 Sheets Plates and Coils, Hastelloy N6022 Sheets Plates and Coils, Alloy C22 Sheets Plates and Coils, and Hastelloy Sheets Plates and Coils. Meanwhile, these Hastelloy Coils are also being offered in customized sizes and shapes to our customers. HASTELLOY C-22 alloy (UNS N06022) is one of the well-known and well-proven nickel-chromium-molybdenum materials, the chief attributes of which are resistance to both oxidizing and non-oxidizing chemicals, and protection from pitting, crevice attack, and stress corrosion cracking.

 

Hastelloy Alloy C22 Plate Specification

 

Product Type

Hastelloy C22 ASTM B575 Sheet, Hastelloy C22 ASTM B575 Plate

Specification

ASTM B575 / ASME SB575

Tolerances (width / thickness)

EN 10258/ DIN 59381)

EN 10151 2.4819 Hastelloy C-22 Strips

EN 10088 Hastelloy C22 SB575 strips

Dimensions

Cold rolled Alloy C22 Plates 0.5-6.4 mm

Hot rolled Alloy C22 Plates 3.0–10.0 mm

Thickness

0.1 to 100 mm Thk

Width

10-2500mm

Length

2m, 2.44m, 3m, or as required

Finish

SATIN, 2B, 2D, BA NO (8), Cold rolled sheet (CR), Hot rolled plate (HR), No.1 finish hot rolled, 1D, No.4, BA, 8K, hairline, brush, mirror etc.

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard

variety of shapes

Coils, Foils, Plates, Sheet, Strip, Plain Sheet, Checker Plates, Rolling Sheet, Flats, Clad Plates, Flat Sheet, Shim Sheet, Rolls, Blank (Circle), Rolling Plates, Flat Shim, soft annealed, descaled, tread Plates, sheared, annealed

 

2.4602 Hastelloy C22 Sheet Composition Chart

 

Grade

C

Mn

Si

S

Co

Ni

Cr

Fe

Mo

P

C22

0.010 max

0.50 max

0.08 max

0.02 max

2.50 max

50.015 min*

20.00 – 22.50

2.00 – 6.00

12.50 – 14.50

0.02 max

 

Mechanical Properties of Hastelloy C22 Plate

 

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Hastelloy C22

8.69 g/cm3

1399 °C (2550 °F)

Psi – 1,00,000 , MPa – 690

Psi – 45000 , MPa – 310

45 %

 

Equivalent Grades Of Hastelloy UNS N06022 Plate

 

STANDARD

WERKSTOFF NR.

UNS

JIS

GOST

EN

OR

Hastelloy C22

2.4602

N06022

NW 6022

NiCr21Mo14W

 

Uses Of ASTM B575 UNS N06022 Plate

 

Incineration scrubber systems

Pharmaceutical industries