Hastelloy C22 Pipe
JN ALLOY supplies Hastelloy C22 Pipe, ASTM B622 UNS N06022 Tube, Hastelloy Alloy C22 Tube, 2.4602 Hastelloy C22 Tube, Hastelloy C22 Tube, Alloy C22 Pipe, Hastelloy C22 Pipe, Alloy C22 Material, Hastelloy C22 Price, DIN 2.4602 Tube, Alloy C22 Tube, Hastelloy C22 Tubing, Alloy C22 Seamless Tubing .
Hastelloy C22 Tubes are preferable austenitic tungsten, molybdenum, chromium, and nickel stabilized alloy tubes with high resistant to the crevice, pitting, stress corrosion cracking. The greater content of chromium alloy is providing excellent resistant to oxidizing media and tungsten and molybdenum alloy is giving well resistant at reducing media. This alloy is having good resistant to the oxidizing aqueous media that is including a mixture that contains oxidizing acid with chlorine ion and wet chlorine. Hastelloy C22 alloy is having a good resistant ability to acetic and formic acid, oxidizing acid chlorides, and other contaminated chemical solutions. This alloy is good at offering greater resistance to an environment where in the reducing, as well as oxidizing conditions, is encountered in the process streams. Hastelloy C22 Seamless Pipe is able to resist corrosion, especially in oxidizing environments as it is able to resist corrosion in aqueous media as well. This particular resistance property of the Hastelloy C22 pipe proves to be rather beneficial to those factories that have upset conditions. More often than not, in chemical processing systems, the pipes need to encounter both reducing and oxidizing conditions (upset) at varying temperature levels.
Jinie Technology (Jiangsu) Co., LTD is one of the prominent manufacturer and supplier of the very good quality of Hastelloy C22 Seamless Tubes. The Hastelloy C22 alloy pipe is designed with superior strength and excellent corrosion resistance properties. These alloys have good wear resistance and can suffice in extreme temperatures and pressures. The Hastelloy C22 material is made with excellent mechanical properties. They possess a minimum tensile strength of 100Ksi and a minimum yield strength of 45ksi. They cater to the needs and requirements of the esteem patrons are providing the tubes in standards specifications as well as in custom made specifications. All our products can be customized as per in different chemical make-up, sizes, and shapes as per the requirements of our clients. We are the Alloy C22 suppliers who make use of the latest technology and best raw materials whilst producing the best products in the market. These products are produced following international and national standards. If you want to know about our products or their pricing contact us to know more.
Hastelloy C22 Pipe and Tubes Specifications
|
Specifications |
ASTM B622, ASME SB622,ASTM B474,ASTM B163 |
|
Standard |
ASTM, ASME, and API |
|
Seamless Pipes& Tubes Size |
1/8"NB--24" NB |
|
Welded Pipes & Tubes Size |
1/8"NB--48" NB |
|
Length |
Single Random, Double Random & Cut Length |
|
Schedule |
SCH 10, SCH20, SCH30, SCH40, STD, SCH60, XS, SCH80, SCH120, SCH140, SCH160, XXS |
|
Types |
Seamless / Welded/ ERW/ EFW / SAW/ SAWL |
|
Form |
Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes |
|
End |
Plain End, Beveled End, Threaded |
Hastelloy C22 Pipes Chemical Composition
|
C≤ |
Cr |
Co≤ |
Fe |
Mn≤ |
Mo |
Ni |
P≤ |
Si≤ |
S≤ |
W |
V≤ |
|
0.015 |
20-22.5 |
2.5 |
2.0-6.0 |
0.50 |
12.5-14.5 |
Balance |
0.02 |
0.08 |
0.02 |
2.5-3.5 |
0.35 |
Hastelloy C22 Pipe Mechanical Properties
|
Element |
Density |
Melting Point |
Tensile Strength,min |
Yield Strength ,min(0.2% Offset) |
Elongation,min |
|
Hastelloy C22 |
8.69 g/cm3 |
1399℃ |
690MPa |
283MPa |
45% |
Hastelloy C22 Tube Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
EN |
|
Hastelloy C22 |
2.4602 |
N06022 |
NW 6022 |
NiCr21Mo14W |
Application field of Hastelloy C22 pipe and tube
Chemical Research Industries
Petroleum and Gas Industries
Agriculture Engineering Industries
Mechanical Engineering Industries
Civil Engineering Industries