Hastelloy B3 plate

 

JN Alloy is largest Stockiest of Hastelloy B3 Plate supplier with huge inventory of Alloy B3 Hot Rolled Plate, ASTM B333 UNS N10675 Polished Plate and Hastelloy B3 Cold Rolled Plate. We offer Din 2.4600 Coils in various sizes at best price. We are leading manufacturer of Alloy B3 strip & Hastelloy B3 Sheet.

 

B3 Hastelloy alloy is molybdenum and nickel alloy that has a good ability to be corrosion resistant, stress corrosion cracking, and pitting, oxidation and crevice corrosion resistance. This property ensures long-term reliability and reduces maintenance costs for equipment and structures. Additionally, it is having high tensile strength, good dimensional accuracy, flexibility, long-lasting, durability that is making fabrication of Hastelloy B3 Sheet & Plate much beneficial. One of the most significant advantages of Hastelloy B3 Sheets and Plates is their exceptional resistance to a wide range of corrosive environments. They perform remarkably well in both reducing and mildly oxidizing environments, making them ideal for industries dealing with aggressive chemicals. Hastelloy B3 Sheets and Plates maintain their mechanical integrity even at elevated temperatures. The combination of corrosion resistance, thermal stability, and mechanical strength ensures that Hastelloy B3 Sheets and Plates have a long service life. This makes them suitable for applications involving high heat, such as heat exchangers, reactors, and other high-temperature equipment. These Hastelloy B3 plates are easy to fabricate, weld, and form into various shapes and sizes. This versatility allows manufacturers to create custom components that meet specific application requirements without compromising performance.

 

JN Alloys are one of the best supplier and stockiest of the very good quality of Hastelloy B3 Sheet & Plate. They are providing the product in wider range so that all application demands can be well satisfied. The product is exported all across the globe in proper condition and at reasonable rates. It is available in different types, sizes, dimensions, thickness so that it can be used easily in the industry for satisfying application demands. our manufactured Hastelloy B3 Sheets & Plates provides resistant to hydrochloric destructive in case and temperatures, it gives a fantastic resistant to setting, provides excellent consumption and uncertain erosion isolate, it provides an excellent resistant to blade line and warmth altered zone invasion. It also shows a superb resistance towards acidic, formic, phosphoric acids, and other non-oxidizing substances. These have excellent mechanical strength and durability to survive in hostile environments. The JN Alloys performs several material tests on Hastelloy B3 Sheet & Plate in order to ensure its strict quality and efficiency before finally delivering it to the customers across the globe.

 

Hastelloy B3 Plate Specification

 

Specifications

ASTM / ASME SB333

Size

1000 mm B3 2000 mm, 1220 mm B3 2440 mm, 1500 mm B3 3000 mm, 2000 mm B3 2000 mm, 2000 mm B3 4000 mm

Thickness

0.1mm to 12 mm Thk

Form

Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Finish

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

 

Hastelloy Alloy B3 Plates Chemical Composition

 

Grade

C

Mn

Si

Cu

Co

Ni

Cr

Fe

Mo

Ti

Hastelloy B3

0.01 max

3.0 max

0.10 max

0.20 max

3.0 max

65.0 min

1.5 max

1.5 max

28.5 max

0.2 max

 

Hastelloy B3 Plates Mechanical Properties

 

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Hastelloy B3

9.2 g/cm3

1370 °C (2550 °F)

Psi – 1,15,000 , MPa –760

Psi – 52,000 , MPa – 350

40 %

 

Hastelloy B3 Plates Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

Hastelloy B3

2.4600

N10675

 

ASTM B575 Hastelloy B3 Plate Application

 

Chemical Processing Industry

Reactors and Equipment: Hastelloy B3 plates are widely used in reactors, vessels, and other equipment exposed to highly corrosive substances like hydrochloric acid.

Heat Exchangers: The alloy's resistance to corrosive environments makes it ideal for heat exchangers where harsh chemicals are processed.

 

Pollution Control

Flue Gas Desulfurization: Hastelloy B3 plate is utilized in flue gas desulfurization systems, where it withstands the corrosive effects of acidic gases and slurries.

Waste Treatment: The alloy is used in equipment for handling and treating industrial waste, where it resists corrosion from harsh chemicals.

 

Marine Engineering

Seawater Applications: Hastelloy B3 plates are employed in marine environments, including seawater cooling systems and desalination equipment, where it is crucial to be resistant to corrosion and high temperatures.

Offshore Structures: The alloy's durability makes it suitable for use in offshore platforms and subsea equipment, ensuring reliability in challenging marine conditions.

 

Oil and Gas Industry

Downhole Equipment: In the oil and gas industry, Hastelloy B3 plate is used for downhole equipment that encounters corrosive fluids and gases, providing long-term performance in harsh environments.

Refinery Components: The alloy is also used in refining processes where it must endure aggressive chemicals and high temperatures.

 

Pharmaceutical Industry

Process Vessels: Hastelloy B3 plates are used in pharmaceutical manufacturing for process vessels that handle corrosive chemicals and need to maintain strict hygiene and safety standards.

Sterilization Equipment: The alloy's resistance to corrosive sterilants makes it suitable for equipment used in the sterilization process.

 