JN ALLOY supplies Hastelloy B3 Pipe, ASTM B622 UNS N10675 Tube, Hastelloy Alloy B3 Tube, 2.4600 Hastelloy B3 Tube, Hastelloy B3 Tube, Alloy B3 Pipe, Hastelloy B3 Pipe, Alloy B3 Material, Hastelloy B3 Price, Alloy B3 Tube, Hastelloy B3 Tubing, Alloy B3 Seamless Tubing.

 

Hastelloy B3 alloy is molybdenum and nickel stabilized alloy addition to the good resistant ability to stress corrosion cracking, pitting and corrosion resisting. Additionally, thermal stability superior is good when compared to other alloys. Hastelloy B3 pipe is made from superalloy with the composition of nickel 65%, and molybdenum 28%. It is best for providing resistance to non-oxidizing acids. Along with tungsten, iron, cobalt, and manganese in small quantities provides thermal stability and is tough in cryogenic temperatures. Hastelloy B3 pipe is having good resistance to knife line as well as the heat affected area. This alloy withstands phosphoric, sulfuric, formic and acetic acid and non-oxidizing media. Additionally, this alloy is having high resistance to hydrochloric acid at various concentrations and temperatures. It too maintains ductility when transient exposure to maintain excellent ductility and is experienced at the time of heat treatment connected with fabrications. Hastelloy B3 pipe has excellent resistance to pitting, corrosion, and cracking due to stress corrosion. It has extra-ordinary resistance to hydrochloric acid at every concentration and range of temperatures.

 

Jinie Technology (Jiangsu) Co., LTD is one of the popular manufacturer, supplier, stockiest and exporter of Hastelloy B3 Pipes. The industry catering to all the needs of buyers are assuring in offering a comprehensive range of Hastelloy B3 pipes. It is easily made available at different specifications, dimensions, grades, standards etc. A buyer seeking to buy it can get at reasonable rates no matters whether the order is placed in huge quantity or in a small amount. Surely the industry will serve their buyers in a better way by offering the quality of value-added and sales after services. Our Hastelloy B3 pipe & tube is produced strictly according to ASTM B622 standard to ensure that the material meets various strict usage requirements. ASTM B622 is a standard specification for nickel-molybdenum alloy seamless pipe & tube, which specifies the requirements for chemical composition, manufacturing process, size, etc. In the manufacture of Hastelloy B-3 seamless pipe & tube & tube, we employ state-of-the-art production techniques. It guarantees the internal and external surface finish, dimensional accuracy and chemical composition of the pipes. In addition, we can also customize the seamless pipe & tube according to customer requirements, including the length and diameter of the pipe.

 

Hastelloy B3 Pipes and Tubes Specification

 

Alloy B3 Pipe Specification

ASTM B 622 ASME SB 622 / ASTM B 619 ASME SB 619

Hastelloy Alloy B3 Pipe Finish

Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF

Alloy B3 Seamless Pipe size

4 to 219mm W. T.: 0.5 to 20mm

Alloy B3 EFW Pipe size

5.0 mm – 1219.2 mm

Test

Hardness Test

Flattening Test

Pitting Resistance Test

Chemical Analysis – Spectro Analysis

Micro and MacroTest

Flaring Test

Intergranular Corrosion (IGC) Test

Mechanical Testing Such as Tensile of Area

Positive Material Identification – PMI Testing

Hastelloy B3 Pipe Form

Hollow, Square, Round, Rectangular , Straight Pipes, Hydraulic Etc.

Alloy B3 Pipe End

Plain End, Beveled End, Treaded.

Hastelloy B3 Pipe Length

Single Random, Double Random & Cut Length.

Hastelloy B3 Pipe Schedule

SCH5, SCH10, SCH40, STD, SCH80, SCH160

Marking

All Hastelloy Alloy B3 Pipes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer's request.)

Hastelloy B3 Welded Pipe size

5.0 mm – 1219.2 mm

Material Test Certificates (MTC)

Material Test Certificates (MTC) as per EN 10204 3.1 and EN 10204 3.2

Specialized in

Large Diameter Alloy B3 Pipe

 

Hastelloy Alloy B3 Tubes Chemical Composition

 

Element

Alloy B3

C

0.01 max

Mn

3.0 max

Si

0.10 max

S

0.03 max

Co

0.20 max

Ni

65.0 min

Cr

1.5max

Fe

15

Mo

28.5

P

0.2 max

 

Hastelloy B3 Tubing Mechanical & Physical Properties

 

Element

Hastelloy Alloy B3

Density

9.2 g/cm3

Melting Point

1370 °C (2500 °F)

Tensile Strength

Psi – 51000 , MPa – 350

Yield Strength (0.2%Offset)

Psi – 1,10,000 , MPa – 760

Elongation

40 %

 

Alloy B3 Tubes Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

Hastelloy B3

2.4600

N10675

 

Application

 

ASTM B474 Hastelloy B3 welded pipes and tubes are used in various high-temperature applications where excellent corrosion resistance, oxidation resistance, and mechanical properties are required. These applications can include industries such as aerospace, chemical processing, power generation, and oil and gas. Hastelloy B3 Pipes and Tubes are preferred for use in aerospace, power generation plant, dental, chemical processing, oil and gas industry, condensers, petrochemicals, pulp, and paper industry, etc.

 