Hastelloy B2 plate

 

JN Alloy is the largest stockist of Hastelloy B2 plate suppliers. We offer DIN 2.4617 coils in various sizes at the best price. We are a leading manufacturer of Hastelloy alloy B2 strip & Hastelloy B2 sheet.

 

Hastelloy B2 plate is a nickel-molybdenum alloy with a high nickel content (approximately 65%). Nickel provides excellent corrosion resistance, while molybdenum enhances the alloy's resistance to pitting, crevice corrosion, and stress corrosion cracking.

 

Alloy 2.4600 Hastelloy B3 Sheet also withstands sulfuric acids and phosphoric acids, along with other non-oxidizing media. ASME SB333 Hastelloy B3 flat sheets maintain ductility even after brief exposure to moderate temperatures.

 

In short, the ASTM B333 Alloy B2 Coil must conform to tensile strength, yield strength, elongation values, and Rockwell hardness. Moreover, the ASTM B333 UNS N10665 sheet, along with the strip, needs to conform to the grain size requirement as mentioned in the specification. Hastelloy B3 alloy plates may be forged as well as hot-worked. This alloy welds well under gas metal arc, gas tungsten arc, and shielded metal arc conditions.

 

JN Alloy is one of the leading manufacturers, supplier and exporters of Hastelloy B2 sheets & plates. We are offering these sheets in a variety of shapes, sizes, dimensions, and thicknesses and also accept customized orders.

 

These Hastelloy N10665 Sheets & Plates provide several benefits and features like rust-free, high durability, and hardness. Our products make it the best-selling in the market with a considerable quantity. Hastelloy B2 offers excellent corrosion resistance and fabricability.

 

JN Alloy is manufacturing Hastelloy 2.4617 sheets & plates by using the high quality of raw material. We focus on offering dimensionally accurate and durable sheets and plates. We are always following the international and national standards and specifications for the highest quality standard.

 

Hastelloy B2 Sheet & Plate Specification

 

Grade

ASTM B333 UNS N10665

Type

Foils, Coils, Plate, Strip, Sheet, Flats, Clad Plate, Rolling Plate, Flat Shim, Plain Sheet, Rolling Sheet Rolls, Blank (Circle), ,Flat Sheet, Shim Sheet, soft annealed, descaled, sheared, annealed, Checker Plate, tread plate

ASTM B333 Alloy B2 Plate surface

BA, No.3, No.4, No.6, No.1, No. 2D, No. 2B, BA NO(8), No.7, 2B, 2D, Hot rolled plate (HR), Cold rolled sheet (CR), No.1 finish hot rolled ASTM B333 Alloy B2 Plate, SATIN (Met with Plastic Coated), 2B, 1D, No.4, 8K, BA, hairline, brush, satin, mirror etc.

ASTM B333 Alloy B2 Plate Length

0-12mm or as required

Alloy B2 Plate Thickness

0.3 to 1200 mm or as required

Hastelloy B2 Plate Width

0-2500mm or as required

UNS N10665 Hastelloy B2 Plate Process

Hot/ Cold Rolled

 

Chemical Composition Of Hastelloy B2 Sheets And Plates

 

Grade

C

Mn

Si

S

Co

Ni

Cr

Fe

Mo

P

Hastelloy B2

0.02 max

1.0 max

0.1 max

0.03 max

1.0 max

Bal

1.0 max

2.0 max

26 – 30

0.04 max

 

Mechanical Properties For Hastelloy B2 Sheets & Plates

 

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

9.2 g/cm3

1370 °C (2500 ºF )

Psi – 1,10,000 , MPa – 760

Psi – 51000 , MPa – 350

40 %

 

Hastelloy B2 Plates Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

EN

Hastelloy B2

2.4617

N10665

NiMo28

 

ASTM B575 Hastelloy B2 Sheets, Plate & Coils Application

 

Hastelloy B2 plates are commonly used in various applications where excellent resistance to reducing environments is required.

 

Chemical processing equipment: Hastelloy B2 plates are known for their great resistance to corrosion. They are often used in chemical processing equipment. This includes reactors, vessels, and piping systems. These systems handle strong chemicals like sulfuric acid, hydrochloric acid, acetic acid, and phosphoric acid.

 

Pollution control: Hastelloy B2 plates are used in pollution control equipment. This includes scrubbers, ducts, and stack liners. They can effectively resist corrosive gases and liquids.

 

Pharmaceutical industry: In pharmaceutical manufacturing, Hastelloy B2 plate are employed in equipment that comes into contact with corrosive chemicals during various processes.

 

Hastelloy B2 plates are used in the petrochemical industry. They are for parts that face tough conditions. These conditions include sulfur compounds, chloride ions, and other harmful substances.

 

Pulp and paper industry: Hastelloy B2 plates are used in equipment like digesters, bleach plants, and evaporators. They resist corrosive chemicals used in production.

 

Hastelloy B2 plates are chosen for their excellent resistance to corrosion. This makes them ideal for many industrial uses.

 

Come To Us
And Start Your RFQs Now.
contact us