Hastelloy B2 Pipe

 

JN ALLOY supplies Hastelloy B2 Pipe, ASTM B622 UNS N10665 Tube, Hastelloy Alloy B2 Tube, 2.4617 Hastelloy B2 Tube, Hastelloy B2 Tube, Alloy B2 Pipe, Hastelloy B2 Pipe, Alloy B2 Material, Hastelloy B2 Price, N10665 Tube, Alloy B2 Tube, Hastelloy B2 Tubing, Alloy B2 Seamless Tubing .


Hastelloy is a superalloy that has excellent tolerances in different environments. The Hastelloy B2 is a nickel, molybdenum alloy which is highly resistant to corrosion and can suffice in extreme conditions. These alloys resists carburization and graining after welding them together. This grade possesses superior strength, and the Hastelloy B2 material used in producing them has excellent mechanical properties. They have a minimum tensile strength of 760Mpa and a minimum yield strength of 350Mpa. Apart from this, they can be easily machined and elongated up to 40%. Hastelloy B2 is actually solid solution strengthened and molybdenum and nickel-based along with significantly resistant to the reducing atmosphere including sulfuric, phosphoric acid etc. here molybdenum alloy is the major element that is providing excellent corrosion resistant to the reducing atmosphere. The nickel steel alloy can be easily used into the welded condition as it is forming grain boundary carbide precipitations at the zone that is heat affected. The nickel alloy is providing good resistant at all temperature and concentrations to the hydrochloric acid. Additionally, this alloy is possessing resistant to SCC and pitting and knife line. It provides a resistant ability to sulfuric acid and several non-oxidizing acids.

 

Jinie Technology (Jiangsu) Co., LTD is one of the prominent manufacturer, supplier and stockiest of the world-class quality of Hastelloy B2 Tubes. The Hastelloy Alloy B2 has excellent resistance against creep rupture and pitting due to acids. These alloys are not advised to be used in oxidizing mediums and in ferric or cupric salts. They are easy to maintain and have a long service life. The Hastelloy B2 Price per kg in India depends on the size, thickness, weight, and color of the material you want. Our experienced workers make use of the latest technology and the best raw materials available in the market to produce the best products. These products are produced following all standards set by various unions with the system. We are the Alloy B2 suppliers who can customize all our products as per your requirements in different shapes and sizes. The product to the buyers are provided at custom made specifications that vary in wall thickness, sizes, dimensions, grades, shapes etc. To all the buyers the product is provided at market leading rates so that ordering in bulk can be easy for them. If you have any queries or want to know more about our products, contact us to know more.
 

Specification Of Hastelloy B2 Pipe & Tube

 

Dimensional :

ASME/ANSI B36.19M, ASME/ANSI B36.10M

Standards :

ASTM B622 , B619/ ASME SB622, SB619

Seamless Pipes Sizes :

1 / 2 to 16 inch NB

Welded Pipes Sizes :

1 / 2 to – 24 inch NB

Outside Dia :

6.00 millimeter OD up to 914.4 millimeter OD

Pipes Type :

Welded / Seamless / ERW / CDW / Fabricated / 100% X Ray Welded

Pipes End :

Plain, Beveled, Threaded One, TBE (Threaded Both Ends)

Thickness Range :

SCH10, SCH 5, SCH 40, SCH 80S, SCH 80, SCH XXS, SCH 160, SCH XS

Value Added Services :

Beveling, Cutting, Polishing, Destructive, Threading, Ultrasonic Testing, Non Destructive

 

Alloy B2 Tube Chemical Composition

 

Hastelloy B2

C

Ni

Mn

Mo

Fe

Si

S

Cr

P

Co

0.02 maximum

Balance

1.0 maximum

26.0-30.0

2.0 maximum

0.10 maximum

0.030 maximum

1.0 maximum

0.040 maximum

1.0 maximum

 

Hastelloy B2 Tubing Mechanical Properties

 

Density

Elongation

Yield Strength (0.2%Offset)

Melting Point

Tensile Strength

9.2 g/cm3

40 %

Psi – 51,000, MPa – 350

1370 °C (2500 °F)

Psi -1,10,000, MPa -760

 

Hastelloy B2 Seamless Pipes Equivalent Grades

 

STANDARDS

WERKSTOFF NR

UNS NO

Hastelloy B2

2.4617

N10665

 

Application field of Hastelloy B2 pipe and tube

 

Food Processing Industry
Fabrication Industry
Oil and Gas Industry
Chemical Industry
Plumbing
General Purpose Applications
Heating
Water Supply Systems
Power Plant
Paper & Pulp Industry
 

Come To Us
And Start Your RFQs Now.
contact us