Duplex steel S32205 plate
JN Alloy is largest Stockiest of Duplex S32205 Plate supplier with huge inventory of AISI S32205 Hot Rolled Plate, ASTM A240 UNS S32205 Polished Plate and Duplex S32205 Cold Rolled Sheets. We offer Din 1.4462 Coils in various sizes at best price. We are leading manufacturer of S32205 steel strip & S32205 duplex stainless steel Sheet.
Duplex steel UNS S32205 is a stainless alloy that combines the properties of both austenitic and ferritic steels. This type of steel is known for its strength, durability, and corrosion resistance in a variety of environments. When it comes to duplex steel UNS S32205 sheets, there are two main types available: cold rolled plates and hot rolled plates. Cold rolled plates are stronger than hot rolled plates as they have undergone additional processing which strengthens them further. Hot rolled plates, on the other hand, are more malleable and easier to form into desired shapes. The high strength grade of Duplex Steel 2205 Plate shows excellent resistance against pitting by acids and crevice corrosion across different stress-induced environments. Duplex Steel S32205 Plates are designed with excellent chemical concentrations of Chromium, Nickel and Molybdenum along with some other elements, these excellent compositions enable these modules to work well in corrosive and oxidizing media. It has excellent general corrosion resistance in a wide variety of corrosive chemicals including seawater and industrial acids.
JN Alloy is enlisted amongst leading manufacturer and supplier of Duplex Steel UNS S32205 Sheets. We are offering this product in different dimensions and technical specifications. We always work to provide the better quality of products to our customers. By following all industrial and International quality standards, we are manufacturing customized as well as non-customized Duplex Steel S32205 Sheets and Plates. These Sheets and Plates are available in different shapes and sizes according to the need and demand of our customers. These Duplex Steel S32205 Plates have to undergo a series of tests so that the products that are produced are of excellent quality and so that they offer outstanding performance.
Duplex Steel S32205 Plate Specifications
|
Specification |
Details |
|
Standard |
ASTM A240 / ASME SA240 |
|
Thickness Range |
5mm to 150mm |
|
Width Options |
1000mm / 1219mm / 1250mm / 1500mm / 2000mm |
|
Length Options |
2000mm / 2440mm / 2500mm / 3000mm / 6000mm |
|
Surface Finishing |
Hot Rolled Plate (HR), Cold Rolled Sheet (CR), 2B, 2D, BA NO(8), Satin (Plastic Coated) |
|
Form |
Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) |
Chemical Structure Of SA 240 S32205 Plate
|
Grade |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
N |
Fe |
|
S32205 |
0.030 max |
2.00 max |
1.00 max |
0.030 max |
0.020 max |
21.0 – 23.0 |
2.50 – 3.50 |
4.50 – 6.50 |
0.8 – 0.20 |
63.54 min |
Mechanical Analysis Of ASTM A240 UNS S32205 Sheet
|
S32205 |
Density |
Melting Point |
Yield Strength (0.2%Offset) |
Tensile Strength |
Elongation |
|
7.8 g/cm3 |
1350 °C (2460 °F) |
Psi – 80000 , MPa – 550 |
Psi – 116000 , MPa – 800 |
15 % |
Applications of Duplex steel SA 240 S32205 Sheet
Chemical process vessels, piping and heat exchangers
Oil field piping and heat exchangers
Pulp mill digesters, bleach washers, chip pre-steaming vessels
Flue gas desulfurization equipment