Incoloy 800H / UNS N08810 / 1.4958

Incoloy 800H / UNS N08810 / 1.4958
Product Introduction:
Type:
Pipes
Plates
Bars
Fittings
Forgings
Flanges
Prefabrication
We are Incoloy 800H manufacturer and supplier, top quality, competitive price, professional distribution and after-sales service team.
Send Inquiry
Description
Technical Parameters

Incoloy 800H characteristics

 

Incoloy 800H(UNS N08810, 1.4958, 1.4876) has good creep-rupture properties at temperatures above 1100°F (600°C). It remains ductile during long term use at temperatures below 1290°F (700°C) due to a maximum titanium and aluminum content of 0.7%. Alloy 800 with a standard anneal is recommended for service below 1100°F (600°C). Alloy 800H resists reducing, oxidizing and nitriding atmospheres, as well as, atmospheres that alternate between reducing and oxidizing. The alloy remains stable in long term high temperature service.

 

Alloy 800H has the following properties

 

1. Excellent corrosion resistance in extremely high temperature aqueous media up to 500°C
2. Good resistance to stress corrosion
3. Good workability

 

Metallographic structure of Incoloy 800H

 

800H is a face-centered cubic lattice structure. Very low carbon content and increased Ti:C ratio increase structural stability and maximum resistance to sensitization and intergranular corrosion. A low-temperature annealing around 950°C ensures a fine-grained structure.

 

Corrosion resistance of Incoloy 800H

 

800H can resist corrosion of many corrosive media. Its high nickel content makes it resistant to stress corrosion cracking in aqueous corrosion conditions. The high chromium content provides better resistance to pitting and crevice corrosion cracking. The alloy has good corrosion resistance to nitric acid and organic acids, but limited corrosion resistance in sulfuric acid and hydrochloric acid. Good corrosion resistance in oxidizing and non-oxidizing salts, in addition to the potential for pitting corrosion in halides. It also has good corrosion resistance in water, steam and mixtures of steam, air and carbon dioxide.

 

The Chemical Composition of Incoloy 800H, %

 

Grade

Ni

Cr

Fe≤

Al

C

Mn

P≤

Si≤

S≤

Al & Ti

Cu≤

Incoloy 800H

30.0-35.0

19.0-23.0

39.5

0.15-0.60

0.05-0.10

1.5

0.045

1.00

0.015

0.30-1.20

0.75

 

Physical Properties of Incoloy 800H

 

Density: 8.0 g/cm3
Melting point: 1350-1400 ℃

 

Incoloy 800H Mechanical Properties

 

Mechanical properties

Tensile, min, ksi[MPa]

Yield, min, ksi[MPa]

Elongation, %(min)

Incoloy 800H

65[450]

25[170]

30

 

Incoloy 800H Equivalent Grades

 

STANDARD

WERKSTOFFNR.

UNS

JIS

BS

GOST

AFNOR

EN

OR

Incoloy 800H

1.4958 / 1.4876

N08810

NCF 800H

NA 15(H)

ЭИ670

Z8NC33-21

X5NiCrAlTi31-20

XH32T

 

ASTM Specifications

 

Product From

Rod and Bar

Plate, Sheet & Strip

Seamless Pipe & Tube

Welded fittings

Forging

Standard

ASTM B408, EN 10095

ASTM A240/ A480/B409/ B906

ASTM B829/ B407

ASTM B366

ASTM B564/DIN 17460

 

Incoloy 800HApplication

 

  • Chemical and Petrochemical Processing-process equipment for theproduction of ethylene, ethylene dichloride, acetic anhydride, ketene,nitric acid and oxy-alcohol.
  • Petroleum Refining-steam/hydrocarbon reformers andhydrodealkylation units.
  • Power Generation-steam super-heaters and high temperature heatexchangers in gas-cooled nuclear reactors, heat exchangers andpiping systems in coal-fired power plants.
  • Thermal Processing Fixtures-radiant tubes, muffles, retorts andfixtures for heat-treating furnaces.

 

 

Hot Tags: incoloy 800h / uns n08810 / 1.4958, China incoloy 800h / uns n08810 / 1.4958 manufacturers, suppliers, alloy for chemical industry, alloy for forging, alloy in green technology, alloy in batteries, alloy in waste treatment, alloy in resource conservation