Alloy 31 plate

 

JN Alloy is largest Stockiest of Alloy 31 Plate supplier with huge inventory of Alloy 31 Hot Rolled Plate, ASTM B463 UNS N08031 Polished Plate and Alloy 31 Cold Rolled Plate. We offer Din 1.4562 Coils in various sizes at best price. We are leading manufacturer of alloy 31 strip & Alloy 31 Sheet.

 

Alloy 31 plate is a nickel, chromium and molybdenum stainless steel with nitrogen and copper additions. This material provides moderate strength and high ductility, combined with excellent resistance to corrosion in sulfuric, phosphoric, and other chemical environments.

 

Alloy 31 (1.4562) in plate form has a smooth, flat surface with uniform thickness. They are available from 3 mm to 50 mm. And it comes with standard widths of 1000 mm or 1219 mm.

 

But Tuolian can offer custom sizes or thicknesses upon your request. Alloy UNS N08031 plates and sheets are also known for excellent weldability and easy fabrication.

 

ASTM B625 UNS N08031 Plate is an iron-nickel-chromium-molybdenum alloy. It has exceptional corrosion resistance to alkaline & halide.

 

JN Alloys is a popular manufacturing company that produces and supplies a wide range of Alloy 31 sheet. We fabricate Alloy 31 plates in various sizes, thicknesses, grades, dimensions, specifications, and types to satisfy clients' diverse demands.

 

We manufacture sheets as per the standard guidelines of national and international industry norms. Our company offers nickel 31 plates with precise dimensions at the most affordable rates. Alloy 31 sheets are a high-performing material that is well-suited to a wide range of applications.

 

Whether you need Nickel 31 Sheet for a chemical processing plant or marine construction, JN Alloys is here for your needs. Contact us today to learn more about our products and services.

 

Nickel Alloy 31 Specification Schedule

 

Specification

ASTM B625, ASME SB 625

Technique

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form

Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Etc.

Surface

2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching

Thickness

0.25-200mm, 0.3mm to 120mm

Width

1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm

Length

2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm

Sizes

 

Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement.

Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt.

Package

Standard Export Seaworthy Package, or as required.

MTC

Mill Test Certificate, Available as per EN 10204 3.1

 

Alloy 31 Chemical Composition

 

The Chemical Composition of Alloy 31, %

Nickel

30.0-32.0

Chromium

26.0-28.0

Iron

Balance

Sulfur

≤0.010

Si

≤0.30

Manganese

≤2.00

Phosphorus

≤0.031

molybdenum

6.0-7.0

Copper

1.0-1.4

Nitrogen

0.15-0.25

Carbon

≤0.015

 

Mechanical Properties of Nickel 31

 

Tensile Strength, min.

Yield Strength, min.

Elongation, min.

Hardness, min

Mpa

ksi

Mpa

ksi

%

HB

650

95

277

41

40

231

 

Alloy 31 Plate Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

EN

Alloy 31

1.4562

N08031

X1NiCrMoCu32-28-7

 

Alloy 31 Plate Application

 

Flue gas desulfurization plants: For handling aggressive gas treatment processes.


Phosphoric acid production: Utilized in wet digestion processes.


Pipes and heat exchangers: For sulfuric acids with chloride contamination.


Water treatment systems: For brackish and ocean water, including condensers and chillers.


Chemical pickling plants: Handling sulfuric, nitric, and hydrofluoric acids.


Paper industry: Resistant to corrosion in chlorine dioxide bleaching plants.


Mineral processing: Used in high-pressure acid leach plants for ore digestion.


Oil and gas industry: Transport and feed pipes for handling harsh environments.


Marine and ship diesel scrubbers: In waste treatment and energy recovery systems.

 

Come To Us
And Start Your RFQs Now.
contact us