904L stainless steel pipe

 

JN Alloy is a distributor and manufacturer that supplies 904L Stainless steel material, 904L stainless steel Pipes and Tubes, ASTM A213 UNS N08904 Tube, 904L Tube, 1.4539 904L Tube, 904L Pipe, 904L Material, 904L Price, 904L Suppliers, N08904 Tube, 904L Tubing.

 

UNS N08904, commonly known as 904L, is a low carbon high alloy austenitic stainless steel. The addition of copper to this grade gives it corrosion resistant properties superior to the conventional chrome nickel stainless steels, in particular to sulphuric, phosphoric and acetic acids. However, there is limited use with hydrochloric acids. It also has a high resistance to pitting in chloride solutions, a high resistance to both crevice and stress corrosion cracking. The stainless steel 904L pipe is non-magnetic in all conditions and has excellent formability and weldability. The austenitic structure also gives this grade excellent toughness, even down to cryogenic temperatures. With the addition of molybdenum, 904L pipes offer enhanced resistance to crevice corrosion, making them perfect for general corrosion applications and moderate to high-temperature conditions. Mechanical tests such as tension and flattening are performed on Stainless steel 904L pipes to ensure strength and durability. These pipes are heat-treated according to ASTM A312 standards for optimal performance.

 

Jinie Technology (Jiangsu) Co., LTD supplies premium 904L stainless steel pipes, known for their high alloy composition and low carbon content. This non-magnetic, austenitic stainless steel 904L pipe contains copper, making it highly resistant to strong acids like sulfuric acid. The low carbon content allows for easier production under ASTM A312 specifications, making it ideal for high-temperature applications. The high chromium content promotes and maintains a passive film which protects the material in many corrosive environments. 904L pipe has a greater resistance to precipitation of ferrite and sigma phases on cooling and welding than other stainless steels containing molybdenum. There is no risk of intercrystalline corrosion on cooling or welding due to the low carbon content. Its maximum service temperature is at 450°C.
 

Standard Specification For Stainless Steel 904L Pipes & Tubes

 

Standards

ASTM / ASME A213, A249, A269, A312, A358 / SA213, SA249, SA269, SA312, SA358

Outer Diameter

6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB

Thickness

0.3mm – 50 mm

Type

Seamless / ERW / EFW / Welded / Fabricated / LSAW Pipes

Schedule

SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS

Seamless Pipes & Tubes Size

1 / 8″ NB – 24″ NB

ERW Pipes & Tubes Size

1 / 8″ NB – 36″ NB

EFW Pipes & Tubes Size

6″ NB – 100″ NB

Length

Single Random, Double Random & Required Length

Form

Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes

End

Plain End, Beveled End, Threaded

 

SS 904L Pipes & Tubes Chemical Composition

 

Grade

C

Mn

Si

P

S

Cr

Mo

Ni

Cu

SS 904L

0.020 max

2.00 max

1.00 max

0.040 max

0.030 max

19.00 – 23.00

4.00 – 5.00 max

23.00 – 28.00

1.00 – 2.00

 

Mechanical Properties of SS 904L Pipes and Tubes

 

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

7.95 g/cm3

1350 °C (2460 °F)

Psi – 71000 , MPa – 490

Psi – 32000 , MPa – 220

35 %

 

Stainless Steel 904L Pipes & Tubes Equivalent Grades

 

STANDARD

WERKSTOFFNR.

UNS

JIS

BS

AFNOR

EN

904L

1.4539

N08904

SUS 904L

904S13

Z1CNDU20.18.06Az

X1NiCrMoCu25-20-5

 

Typical Applications 904L SS Pipes

 

Petrochemical Industry

Oil and Gas Industry

Chemical Industry

Power Plant Industry

Energy Industry

Pharmaceuticals Industry

Pulp & Paper Industry

Food Processing Industry

Aerospace Industry

Refining Industry

 

Come To Us
And Start Your RFQs Now.
contact us