317L Stainless Steel Bars and Rods
JN ALLOY supplies 317L Bars, 317L Rods, UNS S31703 Bars Rods, 1.4438 317L Solid Bars, ASTM A276 UNS S31703 Bars, ASTM A479 Stainless Steel Bars Supplier.
SS 317L Round Bars may contain molybdenum contents of up to 5 % and nitrogen of up to 0.4 %. Stainless Steel 317L Square Bars are magnetic, and offer increased tensile and yield strength over the other categories. When specifying stainless steel chemistry, Stainless Steel 317L Flat Bars is important to reference the appropriate ASTM standard and the UNS (Unified Numbering System) number associated with the specific alloy or grade. UNS numbers of Stainless Steel 317L Threaded Bars are internationally recognized specific chemistry requirements. If common names such as AISI numbers are referenced, the UNS number of Stainless Steel 317L Hollow Bars should also be used to avoid confusion. The many unique values provided by Stainless Steel 317L Hexagonal Bars make it a powerful candidate in materials selection. The bright, easily maintained surface of Stainless Steel 317L Triangular Bars provides a modern and attractive appearance. Engineers and designers often underestimate or overlook these values of Stainless Steel 317L Bars because of what is viewed as the higher initial cost of stainless steel. However, over the total life of a project, Stainless Steel 317L Rods is often the best value option. 317L Stainless Steel Round Bars resist corrosion in atmospheric and pure water environments, while high – alloyed grades can resist corrosion in most acids, alkaline solutions, and chlorine bearing environments, properties which are utilized in process plants.
Stainless Steel 317L Round Bar Specification
|
Specifications |
ASTM A276, ASME SA276 / ASTM A479, ASME SA479 |
|
Dimensions |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
SS 317L Round Bars |
Outside Diameter in the range of 4mm to 500mm |
|
SS 317L Bright Bars |
Outside Diameter in the range of 4mm to 100mm |
|
SS 317L Hex Bars |
18mm – 57mm (11/16″ to 2-3/4″) |
|
SS 317L Square Bars |
18mm – 47mm (11/16″ to 1-3/4″) |
|
SS 317L Flat Bars |
1/2" to 10" in thickness range of 2mm to 150mm, |
|
Finish |
Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
|
Length |
1 to 6 Meters, Custom Cut Lengths |
|
Form |
Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc. |
ASTM A276 AISI 317L Stainless Steel Round Bars Properties
Corrosion Resistance
317L stainless steel rods exhibit remarkable resistance to a wide variety of corrosive media. Their high molybdenum content provides enhanced protection against pitting and crevice corrosion. Whether in chloride - rich environments, such as marine settings, or in chemical processing plants dealing with aggressive chemicals, 317L stainless steel can maintain its integrity. For instance, in seawater desalination plants, the equipment made from 317L stainless steel can withstand the corrosive effects of seawater for long periods, reducing the need for frequent replacements and maintenance.
High - Temperature Resistance
Although 317L stainless steel is not primarily designed for extremely high - temperature applications like some other stainless steels, it can still perform well at moderately high temperatures. It can resist oxidation and maintain its mechanical properties up to a certain temperature range. This makes it suitable for applications where the material is exposed to heat during the manufacturing process or in environments with elevated temperatures.
High Strength
317L stainless steel rods possess good strength and hardness, allowing them to bear significant mechanical loads. In construction projects, especially those in corrosive environments like coastal areas, 317L stainless steel can be used in structural components to ensure the long - term stability and safety of buildings.
Good Processability and Weldability
Despite its excellent performance, 317L stainless steel bar is highly processable. It can be easily shaped using common metal processing techniques like turning, drilling, and milling. Regarding welding, methods such as gas tungsten arc welding (GTAW) and gas metal arc welding (GMAW) are suitable for 317L stainless steel. After welding, the material can still retain its properties, ensuring the structural integrity of the welded components. The following table shows some performance parameters of 317L stainless steel bar:
|
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
8.0 g/cm3 |
1400 °C (2550 °F) |
Psi – 75000, MPa – 515 |
Psi – 30000, MPa – 205 |
35 % |
Types of Stainless Steel 317L Bars / Rods
|
Stainless Steel 317L Bright Bar |
SS 317L Bright Bar |
|
Stainless Steel 317L Hex Bar |
SS 317L Hex Bar |
|
Stainless Steel 317L Square Bar |
SS 317L Square Bar |
|
Stainless Steel 317L Rectangular Bar |
SS 317L Rectangular Bar |
|
Stainless Steel 317L Flat Bars |
SS 317L Flat Bar |
|
Stainless Steel 317L Polished Bar |
SS 317L Polished Bar |
|
Stainless Steel 317L Threaded Bar |
SS 317L Threaded Bar |
SS 317L Round Bar Technology
Although 317L stainless steel is not the easiest to machine, it can be done successfully with the right techniques. Use sharp, carbide-tipped tools, operate at lower speeds with higher feeds, and employ plenty of coolants to reduce heat buildup and improve tool life. To ensure the welded joints maintain the same level of corrosion resistance as the base material, it is essential to use appropriate filler materials. Use AWS E317L/ER317L fillers to match the base metal composition. Additionally, austenitic, low-carbon fillers with higher molybdenum content than Type 317L, or nickel-base fillers with sufficient chromium and molybdenum, can be used to enhance the weld's properties. 317L stainless steel can be easily formed through cold working techniques like drawing and stamping, which maintain its mechanical properties, and hot working processes such as forging and rolling, with a recommended temperature range of 927°C to 1204°C (1700°F to 2200°F). Rapid cooling after hot working is necessary to retain the steel's corrosion resistance. We rovide precise and clean cuts, suitable for complex shapes. Methods such as shearing and sawing are effective but require care to prevent overheating in the heat-affected zone, which could compromise corrosion resistance. Using carbide or high-speed steel tools and maintaining lower cutting speeds are recommended.
Weight Chart of ASME SA276 Stainless steel 317L Square Bar
|
Diameter or |
Weight per meter |
Sectional Area |
Perimeter |
|||
|
Square |
Round |
Square |
Round |
Square |
Round |
|
|
5.0 |
0.20 |
0.15 |
0.25 |
0.20 |
2.0 |
1.57 |
|
5.5 |
0.24 |
0.19 |
0.30 |
0.24 |
2.2 |
1.78 |
|
6.0 |
0.28 |
0.22 |
0.36 |
0.28 |
2.4 |
1.88 |
|
7.0 |
0.38 |
0.30 |
0.49 |
0.38 |
2.8 |
2.20 |
|
8.0 |
0.50 |
0.39 |
0.64 |
0.50 |
3.2 |
2.51 |
|
9.0 |
0.64 |
0.50 |
0.81 |
0.64 |
3.6 |
2.83 |
|
10 |
0.73 |
0.63 |
1.00 |
0.79 |
4.0 |
3.14 |
|
11 |
0.95 |
0.75 |
1.21 |
0.95 |
4.4 |
3.46 |
|
12 |
1.13 |
0.89 |
1.44 |
1.13 |
4.8 |
3.77 |
|
14 |
1.54 |
1.21 |
1.96 |
1.54 |
5.6 |
4.40 |
|
16 |
2.01 |
1.58 |
2.56 |
2.01 |
6.4 |
5.03 |
|
18 |
2.54 |
2.00 |
3.24 |
2.54 |
7.2 |
5.65 |
|
20 |
3.14 |
2.47 |
4.00 |
3.14 |
8.0 |
6.28 |
|
22 |
3.80 |
2.98 |
4.84 |
3.80 |
8.8 |
6.91 |
|
25 |
4.91 |
3.85 |
6.25 |
4.91 |
10.0 |
7.85 |
|
28 |
6.15 |
4.83 |
7.84 |
6.16 |
11.2 |
8.80 |
|
32 |
8.04 |
6.31 |
10.24 |
8.04 |
12.8 |
10.05 |
|
36 |
10.17 |
7.99 |
12.96 |
10.18 |
14.4 |
11.31 |
|
40 |
12.56 |
9.86 |
16.00 |
12.57 |
16.0 |
12.57 |
|
45 |
15.90 |
12.49 |
20.25 |
15.90 |
18.0 |
14.14 |
|
50 |
19.62 |
15.41 |
25.00 |
19.64 |
20.0 |
15.71 |
|
56 |
24.62 |
19.34 |
31.36 |
24.63 |
22.4 |
17.59 |
|
63 |
31.16 |
24.47 |
36.69 |
31.17 |
25.2 |
19.79 |
|
71 |
39.57 |
31.08 |
50.41 |
39.59 |
28.4 |
22.31 |
|
80 |
50.24 |
39.46 |
64.00 |
50.27 |
32.0 |
25.13 |
Application Of Stainless Steel 317L Round Bar
Pharmaceutical Industry
The pharmaceutical industry demands materials that are hygienic, corrosion - resistant, and easy to clean. 317L stainless steel bars are widely used in the manufacture of equipment such as reactors, storage tanks, and pipelines. Their smooth surface and excellent corrosion resistance prevent the contamination of pharmaceutical products and ensure compliance with strict industry standards.
Marine Industry
In the marine environment, materials are constantly exposed to saltwater, which is highly corrosive. 317L stainless steel bars are used in shipbuilding, for components like deck fittings, propeller shafts, and seawater piping systems. Their resistance to chloride - induced corrosion makes them an ideal choice for withstanding the harsh marine conditions. ### Chemical Industry Similar to 310S stainless steel, 317L stainless steel bars are also used in the chemical industry. They are employed in the production of chemical reactors, heat exchangers, and storage vessels for handling corrosive chemicals. Their ability to resist a wide range of chemical substances ensures the long - term operation of chemical plants.
Food and Beverage Industry
The food and beverage industry has strict requirements for material hygiene and corrosion resistance. 317L stainless steel rods are used to manufacture food processing equipment, such as conveyor belts, mixing tanks, and beverage production lines. Their non - toxic nature, smooth surface, and resistance to corrosion make them suitable for ensuring food safety and quality. 317L stainless steel bars play a vital role in the industrial world due to their outstanding performance, well - developed production technology, and extensive application areas. As industrial technology continues to progress, 317L stainless steel bars are expected to find even more applications and contribute to the growth of various industries.