316H Stainless steel pipe
316H Stainless Steel Pipes, 316H Stainless Steel Tubes, 316H Stainless Steel Seamless Pipe & Tubes, 316H Stainless Steel Welded Pipes and Tubes, 316H Stainless Steel Tubing, UNS S31609 Pipes and Tubes, 1.4919 Stainless Steel Pipes & Tubes.
Alloy 316H is an alloy that is high carbon modification of 316 that is developed for use at the elevated temperature services. The alloy is having high strength at an elevated temperature and is used for certain applications at 500 Deg C. The high carbon content at stainless steel 316H is delivering high yielding and high tensile strength than other alloys. The austenitic structure is providing greater toughness down to the cryogenic temperature.
The alloy corrosion resistance is comparable to other alloys and is also superior in nature at the moderately oxidizing as well as reducing the atmosphere. It is also resisting corrosion at polluted marine atmosphere. SS 316H tubes are non-magnetic in nature at annealed atmosphere and can be welded easily. The Stainless Steel 316h Square Pipe is used in structures where strength is the foremost concerns whereas high temperatures are also involved. Applications such as heat exchangers, boilers, power plants and hot water and steam applications can use the A312 Tp 316h given that the sulfur gases are absent.
Jinie Technology (Jiangsu) Co., LTD is one of the top leading manufacturer, supplier, and exporter of the high quality of Stainless Steel 316H Tubes. They are manufacturing and offering it in both welded and seamless construction. Stainless Steel 316H tubes are fabricated using quality of stainless steel tubes at different specifications, standards, and dimensions. It is made easily available at custom made shapes, sizes, wall thickness according to the prerequisites of the buyers. Our ASTM A312 Tp 316h are of superior quality and always test the products under international standard guidelines. Please contact us for further information of the products and pricing.
Standard Specification For Stainless Steel 316H Pipes & Tubes
|
Standards |
ASTM / ASME A213, A249, A269, A312, SA213, SA249, SA269, SA312, |
|
Outer Diameter |
6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB |
|
Thickness |
0.3mm – 50 mm |
|
Type |
Seamless / ERW / EFW / Welded / Fabricated / LSAW Pipes |
|
Schedule |
SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
|
Seamless Pipes & Tubes Size |
1 / 8″ NB – 24″ NB |
|
ERW Pipes & Tubes Size |
1 / 8″ NB – 36″ NB |
|
EFW Pipes & Tubes Size |
6″ NB – 100″ NB |
|
Length |
Single Random, Double Random & Required Length |
|
Form |
Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Hydraulic Tubes |
|
End |
Plain End, Beveled End, Treaded |
Stainless steel 316H Pipes & Tubes Chemical Composition
|
Grade |
UNS |
C≤ |
Mn |
P≤ |
S≤ |
Si≤ |
Cr |
Ni |
|
316H |
0.04--0.10 |
0.75 |
2.00 |
0.045 |
0.030 |
16.00--18.00 |
2.00--3.00 |
10.00--14.00 |
Stainless steel 316H Pipes and Tubes Mechanical Properties
|
Mechanical properties |
Tensile, min, ksi[MPa] |
Yield, min, ksi[MPa] |
Elongation, %(min) |
Hardness, HB(max) |
|
316H |
205 |
515 |
40 |
217 |
SS 316H Pipes & Tubing Equivalent Grades
|
STANDARD |
UNS |
EN |
WERKSTOFF NR. |
|
316H |
S31609 |
X6CrNiMO17-13 |
1.4919 |
316H Stainless Steel Pipes and Tubes Applications
Chemical equipment: due to its corrosion resistance and high-temperature strength, 316H is commonly used in the manufacture of chemical equipment, including reactors, distillation towers, reactors and so on.
Oil and gas industry: In oil and gas processing, 316H stainless steel can be used in the manufacture of pipelines, valves, tanks and other equipment to cope with corrosive media and high-temperature environments.
Nuclear power plant: as one of the materials for key components in nuclear power plants, 316H stainless steel is widely used in nuclear reactor pressure vessels, heat exchangers, piping systems and so on.
Chemical processing: in the chemical industry, 316H stainless steel is often chosen to manufacture chemical reactors, evaporators, extractors and other equipment that need to withstand corrosive media and high temperatures.