316 Stainless steel pipe

 

316 Stainless Steel Pipes, 316 Stainless Steel Tubes, 316 Stainless Steel Seamless Pipe & Tubes, 316 Stainless Steel Welded Pipes and Tubes, 316 Stainless Steel Tubing, UNS S31600 Pipes and Tubes, 1.4401 Stainless Steel Pipes & Tubes, 1.4436 Stainless Steel Pipes and Tubes.

 

Stainless Steel 316 Pipe is an austenitic stainless steel grade pipe that has good resistance to chloride ion corrosion stress cracking. The Stainless Steel 316 Pipe is designed with excellent corrosion resistance. These grade has better crevice corrosion and pitting resistance compared to the 304 alloys. The Stainless Steel 316 Tube is designed with a minimum tensile strength of 515Mpa and minimum yield strength of 200Mpa. They also possess a good density of 8000kg/m3. The standard wall thickness of these tubes ranges from 0.5mm to 6.35mm. The SS 316 Seamless Pipe is made without a fillet or welds. These pipes range from ½ inches to 16 inches in outer diameter. They are widely used in marine systems, pulp, and paper, chemical industries, etc. This Marine grade 316 Stainless Steel Tubing doesn't corrode or rust in these harsh marine environments. It is also referred to in many cases as marine stainless steel.

 

Jinie Technology (Jiangsu) Co., LTD are the leading stockist of Stainless Steel 316 Pipe. Our vision is focused on providing the best products at reasonable rates. Stainless 316 Pipe, constructed to meet ASTM A312 standards for both welded and seamless varieties, epitomizes excellence and durability. With dimensions adhering to ASME B36.19, B36.10, and A276 specifications, our pipe ensures precise fit and compatibility for various applications. Manufactured under ISO 9001:2008 certification, we uphold stringent quality standards. For this reason, the pipe is used in marine and sea water applications with ease. Jinie Technology (Jiangsu) Co., LTD is a leading supplier and manufacturer of the Stainless Steel 316 Pipe products in various scales and dimensions.

 

Standard Specification For Stainless Steel 316 Pipes & Tubes

 

Standards

ASTM / ASME A213, A249, A269, A312, SA213, SA249, SA269, SA312,

Outer Diameter

6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB

Thickness

0.3mm – 50 mm

Type

Seamless / ERW / EFW / Welded / Fabricated / LSAW Pipes

Schedule

SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS

Seamless Pipes & Tubes Size

1 / 8″ NB – 24″ NB

ERW Pipes & Tubes Size

1 / 8″ NB – 36″ NB

EFW Pipes & Tubes Size

6″ NB – 100″ NB

Length

Single Random, Double Random & Required Length

Form

Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Hydraulic Tubes

End

Plain End, Beveled End, Treaded

 

Stainless steel 316 Pipes & Tubes Chemical Composition

 

Grade

UNS

C≤

Mn

P≤

S≤

Si≤

Cr

Ni

TP316

S31600

0.08

2

0.045

0.03

1

16.0-18.0

2.00-3.00

 

Stainless steel 316 Pipes and Tubes Mechanical Properties

 

Mechanical properties

Tensile, min, ksi[MPa]

Yield, min, ksi[MPa]

Elongation, %(min)

Hardness

Rockwell B (HR B) max

Brinell (HB) max

TP316

75【515】

30【205】

35

95

217

 

SS 316 Pipes & Tubing Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

BS

GOST

AFNOR

EN

316

1.4401/1.4436

S31600

SUS316

316S31 / 316S33

-

Z7CND17‐11‐02

X5CrNiMo17-12-2 / X3CrNiMo17-13-3

 

316 Stainless Steel Pipes and Tubes Applications

 

These numerous advantages and benefits mean that 316 Stainless Steel pipe is used in many different applications and environments which include the following examples:

 

Food preparation surfaces, equipment, and appliances, particularly in chloride environments

Laboratory benches & equipment

Coastal architectural panelling, railings & trim

Boat fittings

Chemical containers, including for transport

Heat Exchangers

Woven or welded screens for mining, quarrying & water filtration

Structural steel and components in marine environments

Medical equipment

 

Come To Us
And Start Your RFQs Now.
contact us