310S Stainless steel pipe

 

Jinie Technology (Jiangsu) Co., LTD is a distributor and manufacturer that supplies 310S Stainless steel material, 310S stainless steel Pipes and Tubes, ASTM A213 UNS S31008 Tube, 310S Tube, 1.4845 310S Tube, 310S Pipe, 310S Material, 310S Price, S31008 Tube, 310S Tubing.

 

310S Stainless Steel Pipe is superior than 304 or 309 stainless steel in most environments, because it has high nickel and chromium content with low carbon content. It has high corrosion resistance and strength in temperatures up to 1149°C (2100°F). Stainless Steel 310s grade pipes are widely used in various industries due to their ability to withstand high temperatures and resist corrosion in different environmental conditions. These pipes are low carbon grade alloys that can intermittently withstand temperatures up to 1050 degrees Celsius. Although the austenitic heat-resistant alloy helps these pipes to resist oxidation and corrosion at very high temperatures, they are mainly used in the heat treatment and process industries.

 

Jinie Technology (Jiangsu) Co., LTD offers various sizes, forms, and varieties Stainless Steel 310s pipes are available in welded, seamless, fabricated, and other conditions, as well as multiple shapes such as round, square, rectangular, pancake, hydraulic, 'U' shape, and coil. These pipes are almost the same thickness and size as other grades of this material. They are commonly used in construction, ships, weaponry, vehicles, tools, machinery, condensers, the pulp and paper industries, pharmaceuticals, petrochemicals, and other applications. All products are thoroughly tested according to industry standards. Quality checks include hardness testing, flattening tests, flaring tests, pitting tests, and intergranular corrosion tests before the products are supplied to the final client.

 

Standard Specification For Stainless Steel 310S Pipes & Tubes

 

Standards

ASTM / ASME A213, A249, A269, A312, A358 / SA213, SA249, SA269, SA312, SA358

Outer Diameter

6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB

Thickness

0.3mm – 50 mm

Type

Seamless / ERW / EFW / Welded / Fabricated / LSAW Pipes

Schedule

SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS

Seamless Pipes & Tubes Size

1 / 8″ NB – 24″ NB

ERW Pipes & Tubes Size

1 / 8″ NB – 36″ NB

EFW Pipes & Tubes Size

6″ NB – 100″ NB

Length

Single Random, Double Random & Required Length

Form

Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes

End

Plain End, Beveled End, Threaded

 

SS 310S Pipes & Tubes Chemical Composition

 

Grade

C

Mn

Si

P

S

Cr

Mo

Ni

N

SS 310S

0.08 max

2.0 max

1.00 max

0.045 max

0.030 max

24.00 – 26.00

0.75 max

19.00 – 21.00

53.095 min

 

Mechanical Properties of SS 310S Pipes and Tubes

 

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

7.9 g/cm3

1402 °C (2555 °F)

Psi – 75000 , MPa – 515

Psi – 30000 , MPa – 205

40 %

 

310S Stainless Steel Pipes and Tubes Physical Properties

 

Grade

Density (kg/m3)

Elastic Modulus (GPa)

Mean Coefficient of Thermal Expansion(μm/m/°C)

Thermal Conductivity(W/m.K)

Specific Heat 0-100°C (J/kg.K)

Electrical Resistivity (nΩ.m)

0-100°C

0-315°C

0-538°C

at 100°C

at 500°C

310 / 310S

7750

200

15.9

16.2

17.0

14.2

18.7

500

720

 

Stainless steel 310S Pipes & Tubes Mechanical Properties

 

Grade

Tensile, min, ksi[MPa]

Yield, min, ksi[MPa]

Elongation, %(min)

Hardness, HB(max)

310S

75【515】

30【205】

40

192

 

Stainless steel 310S Pipes & Tubes Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

GOST

EN

BS

310S

1.4845

S31008

SUS310S

20Ch23N18

X8CrNi25-21

310S16

 

Application fields of 310S stainless steel tube

 

310S stainless steel tube has a wide range of applications in many fields, mainly including the following aspects:

Chemical industry: 310S stainless steel tube has good corrosion resistance and can resist the erosion of acid and alkali media. It is often used in chemical pipelines, storage tanks, and equipment.

 

Petroleum industry: In the links of petroleum extraction, refining, and oil transportation, 310S stainless steel tube withstands high temperature and high-pressure working environments and has good corrosion resistance and wear resistance.

 

Energy industry: used to manufacture boilers, heat exchangers gas pipelines, etc. 310S stainless steel pipes can withstand working conditions under high temperatures and high pressure to ensure the safe and stable operation of equipment.

 

Building decoration: 310S stainless steel pipes have good decorative and weather resistance and are often used for indoor and outdoor decoration, railings, and stair handrails.

 