254SMO Stainless steel pipe

 

Jinie Technology (Jiangsu) Co., LTD is a distributor and manufacturer that supplies 254smo Stainless steel material, 254smo stainless steel Pipes and Tubes, ASTM A213 UNS S31254 Tube, 1.4547 254smo Tube, 254smo Pipe, 254smo Material, 254smo Price, S31254 Tube, 254smo Tubing.

 

Stainless steel 254 SMO is an austenitic stainless steel with a high molybdenum content. Coupled with Nickel and Copper this gives the alloy a good resistance to pitting and crevice corrosion, especially in environments containing halide ions, e.g. chloride, bromide and fluoride solutions. 254 SMO (UNS S31254) may offer a cost effective solution to Nickel and Titanium alloys in these environments.

 

254 SMO pipes offer numerous advantages over traditional metal piping options, efficient to their superior corrosion resistance and strength at high temperatures. The main benefit of using 254 SMO pipes is their superior corrosion resistance compared to other grades of stainless steel. This makes them the ideal choice for highly corrosive environments where other materials may not be able to withstand harsh conditions without degrading or failing prematurely. These features make them well-suited for a wide range of industries, including chemical processing plants, oil refineries, power generation plants, and marine engineering projects where exposure to highly corrosive substances is common place. Stainless steel 254 SMO pipes are exceptional industrial components known for their high resistance to corrosion, pitting, and crevice corrosion due to their superior alloy composition.

 

An ISO 9001:2008 Certified Company, Jinie Technology (Jiangsu) Co., LTD is a leading stockholder, supplier and exporter of 254 SMO Pipes. 254 SMO Pipes come in various dimension to suit the requirement of our clients and supplied with complete set of mill test reports. Exports is Our Specialty! and we can source many hard to find grades and or non-standards sizes to meet the special requirements of our customers. Our excellent goods and services have impressed customers not only in India, but also in other countries.
 

Standard Specification For Stainless Steel 254SMO Pipes & Tubes

 

Standards

ASTM / ASME A213, A249, A269, A312, A358 / SA213, SA249, SA269, SA312, SA358

Outer Diameter

6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB

Thickness

0.3mm – 50 mm

Type

Seamless / ERW / EFW / Welded / Fabricated / LSAW Pipes

Schedule

SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS

Seamless Pipes & Tubes Size

1 / 8″ NB – 24″ NB

ERW Pipes & Tubes Size

1 / 8″ NB – 36″ NB

EFW Pipes & Tubes Size

6″ NB – 100″ NB

Length

Single Random, Double Random & Required Length

Form

Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes

End

Plain End, Beveled End, Treaded

 

Chemical Composition of SMO 254 Stainless Steel Pipes and Tubes

 

C

Si

Mn

P

S

Cr

Ni

Mo

N

Cu

≤0.020

≤0.80

≤1.00

≤0.030

≤0.010

20

18

6.1

0.20

0.7

 

Mechanical Properties of SMO 254 Stainless Steel Pipes and Tube

 

Properties

Metric

Imperial

Tensile strength

680 MPa

98600 psi

Yield strength

300 MPa

43500 psi

Modulus of elasticity

195 GPa

28300 ksi

Shear modulus

75 GPa

10900 ksi

Poisson's ratio

0.30

0.30

Elongation at break

50 %

50 %

Hardness, Brinell

210

210

 

Stainless steel 254SMO Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

AFNOR

EN

SMO 254

1.4547

S31254

Z1 CNDU20.18.06AZ

X1CrNiMoCuN20-18-7

 

ASTM A312 UNS S31254 Stainless Steel Pipes and Tubes Applications

 

Petrochemical Industry
Oil and Gas Industry
Chemical Industry
Power Plant Industry
Energy Industry
Pharmaceuticals Industry
Pulp & Paper Indusry
Food Processing Industry
Aerospace Industry
Refining Industry
 

Come To Us
And Start Your RFQs Now.
contact us